FUFINI 微水泥全方位解析:特性、施工与养护指南

微水泥防水吗?

Is microcement waterproof?

 

1)双组分微水泥(粉末+树脂):  

材料本身具有防水性。  

 

1)Two-Component Microcement(Powder + Resin):

Inherently waterproof throughout the material. 

 

2)单组分微水泥(粉末+水/预混膏体):  

默认不具备防水性。  

防水处理:需添加A+B防护面漆作为密封层以实现防水。

 

2)Single-Component Microcement (Powder + Water / Pre-mixed Paste):

Not waterproof by default

Waterproofing: Achieved by adding Protective Topcoat A+Bas a sealing layer.

 

 

 

微水泥防滑吗?

Is microcement slip-resistant?

 

是的,防滑等级:P4  

对于商业区域或住宅浴室:要求防滑等级达到P4至P5。  

 

Yes,anti-Slip Rating:P4

For Commercial Areas or Residential Bathrooms: A slip resistance level of P4 to P5 is required.

 

 

 

 

微水泥和抛光混凝土有什么区别?

What are the differences between microcement and polished concrete?

 

1)施工更快更简便。  

无需使用机械或重型工具进行安装。

 

1)Faster and easier to apply.

It does not require machinery or heavy tools for its installation.

 

2)工序更少、成本更低、耗时更短。  

质地更轻,因此不会产生结构负荷。

  

2)Less work. Less cost. Less time.

Lighter, so there are no structural loads.

 

3)可用于任何房间,而非仅限于底层。  

无需接缝,干燥时不会出现裂缝。  

可应用于水平和垂直表面。

 

3)Use in any room, not just ground floors.

It doesn't need joints, and no cracks appear when drying.

It can be applied both on horizontal and vertical surfaces.

 

 

 

用微水泥进行的翻新工程能维持多久?

How long does a renovation with microcement last?

 

1)工期:  

墙面/天花板:3-5天。  

地面:最多1周(因需养护和密封处理)。  

 

 

2)为何施工快速?  

 

无需拆除:可直接在现有表面上施工。  

薄层施工(2-3毫米),干燥速度快。

 

 

门需要刷漆吗?

Is it necessary to brush the doors?

 

无需刨门  

微水泥仅使地面增厚1 - 3毫米。  

标准门底间隙为5毫米,留有充足空间  。

 

No Need to Plane Doors 

Microcement adds only 1-3mm thicknessto floors.

Standard door clearance is 5mm, leaving enough space.

 

 

3)颜色/纹理/是否容易变色/与其他材料搭配效果如何

3) Color / Texture / Tendency to Discolor / How is the Matching Effect with Other Materials

 

瓷化涂料有100个标准色,3个光泽度,6种标准质感,可定制任意颜色和部分特殊纹理,耐用十五年不变色,可以与液态石材和微水泥搭配,节省施工成本,缩短完工日期

 

The porcelainized coating has 100 standard colors, 3 levels of gloss, and 6 standard textures. Any color and some special textures can be customized. It will not fade within 15 years of use. It can be matched with liquid stone and micro-cement, which can save construction costs and shorten the completion date.

 

 

 

 

如何清洁FUFINI微水泥?

How to Clean FUFINI Microcement?

 

1)简易清洁方法:使用水加中性肥皂。

步骤:

用湿抹布或拖把擦拭。

用软毛巾擦干。

 

1)Simple Solution: Usewater + neutral pH soap.

Steps:

Wipe with a damp cloth/mop.

Dry with a soft towel.

 

2)避免使用:刺激性化学品、漂白剂或研磨性工具。

 

2)Avoid: Harsh chemicals, bleach, or abrasive tools.

 

 

 

微水泥会随时间褪色吗?

Can microcement lose color over time?

 

1)久用不褪色

稳定色素:FUFINI微水泥的色彩可多年保持原本的鲜亮。

耐候性强:抗紫外线、耐潮湿,且能抵御温度变化。

 

1)No Fading Over Time 

Stable Pigments: FUFINI microcement colors retain their original vibrancy for years.

Weatherproof: Resistant to UV rays , humidity , and temperature changes.

 

2)为何经久耐用

优质材料:采用抗褪色矿物和树脂调配而成。

密封

 

2)Why It Lasts ️

High-Quality Materials: Formulated with fade-resistant minerals and resins.

Sealed Protection: Optional UV-resistant sealers enhance longevity.

 

 

 

 

为什么FUFINI微水泥样品与最终成品的光泽度可能存在差异

Why FUFINI Microcement Samples vs. Final Work May Differ in Shine 

 

1)手工施工

自然差异:微水泥采用手工涂抹,因此材料厚度、施加的压力以及工具使用技巧可能会使光泽度产生细微差异。

 

1) Handcrafted Application 

Natural Variations: Microcement is applied manually, so material thickness, pressure, and tool techniques can slightly alter gloss levels.

 

2)材料用量与工具

材料用量:涂层较厚可能会降低光泽度;涂层较薄则会增强光泽度。

工具选择:刷子、滚筒或抹子会影响表面质感和反光度。

 

2)Material Load & Tools

Material Amount: Thicker layers may reduce shine; thinner layers enhance gloss.

Tool Choice: Brushes, rollers, or trowels affect texture and reflectivity.

 

3)光线与环境

自然光或人造光的照射角度可能会使相同的饰面显得更亮或更暗。

 

3)Lighting & Environment 

      Natural/artificial light angles can make the same finish appear brighter or duller.

 

 